What is the difference between duplex 2205 and 2507?

Super Duplex S32750 Steel Pipe

Duplex 2205 and 2507 are both duplex stainless steels with high levels of corrosion resistance and strength. However, there are differences between the two:

1. Chemical composition: Duplex 2205 has a lower percentage of alloying elements such as nickel and molybdenum than 2507. 2205 contains 22 percent chromium, 3 percent molybdenum, and 4.5-6.5 percent nickel, while 2507 contains 25 percent chromium, 4 percent molybdenum, and 7 percent nickel.

2. Corrosion resistance: Super duplex 2507 pipe2205 duplex stainless steel

3. Strength: 2507 has higher tensile and yield strength than 2205, making it more suitable for applications that require high strength.

4. Price: Due to its higher alloy content and better performance, 2507 is more expensive than 2205.

Overall, both duplex stainless steels pipe offer excellent corrosion resistance and strength, but 2507 pipe is a superior choice for applications where corrosion resistance is critical.

 

 